Yes, fiberglass dust is very harmful to breath.
Explanation
This is a quiz over module 4 text and the resources. Body Fillers and Fiberglass Fillers
If there are streaks showing, the filler is not properly mixed. Keep mixing until one uniform color.
This is one of the most important steps to achieving a level surface.
When using a block, the guide coat will help you identify the highs and lows.
Surface must be metal or sanded epoxy. Finish glaze can be applied over sanded paint surfaces.
Cream hardener will separate in the tube. You should kneed (mix) it in the tube before using.
Several thin coats will produce better results than one thick coat. Remember to apply a tight coat first followed by a fill coat.
A tight coat assures proper adhesion.
Larger dent use what will work the fastest with the least amount of effort. 36 grit works good to level followed by 80 to minimize the 36 scratches. Then 150 grit can be used to minimize the 80 grit scratches. Some painters prefer to use 180 grit or 220 grit rather than 150 grit.
Bondo is just a brand name of body filler.
Finish glaze can be applied over sanded paint, body filler or metal. However, the surface should be sanded with 180 grit or courser before applying the glaze.
Causes air bubbles, which will lead to pinholes after sanded.
24 to 50 grit on a grinder or 36 to 80 grit on a DA sander. 220 to 320 is used for block sanding and feather edging.
Any section locations that will show should use fiberglass or aluminum filler should be applied to seal the weld location for corrosion protection. Then the repair can be finished with body filler.
Golf ball of filler to a dime size of hardener is the general rule.
You should not use cardboard to mix body filler. You should use a non-porous surface such as plastic, metal or glass.
Fiberglass seals well, but is harder to sand than body filler.
Some technicians claim that using a rag between their hand and the surface helps them feel highs and lows.
Fiberglass filler is used over welded areas to seal to prevent corrosion from occurring.
Finish glaze is not less expensive than body filler. It is more expensive.
The 3M Dynamic Mixing system is a tool used to mix body filler.
That is regular fiberglass. Fiberglass filler comes in a can much like body filler.